![](https://blogger.googleusercontent.com/img/b/R29vZ2xl/AVvXsEjdkSDp43q2f-xsK8hWk1eUAEaO8bSqSeAAh1KkCh5_accc1iYNPP2OZOcyYz7iD4k3rTrnInK887mRKbA3hlRSoNWjToFDL0JXBTK9C4P6i16PBYK70uX2Ur3Lf0KOWOf4Ga7_vvYSFuQt/s320/Rust+before+%2526+after.jpg)
Here's some before and after pics I took after leaving these parts in the Molasses from Thursday night to Monday morning. I pulled the parts out of the solution and hosed them off and gave them a quick scouring with a wire brush and there was bare metal and original paint! I noticed that after a few minutes the parts began to "flash rust" I wasn't too surprised since I'd read about that happening. So I brushed off the parts again, rinsed dried and sprayed them down with "Rustoleum Automotive Rust Preventing Primer" so that they wouldn't re-rust. More to come!